Barium carbonate can be used to precipitate the salts inside the clay matrix so they do not come to the surface on drying.
Ceramic soluble salts.
When soluble salts are present within the ceramic structure at a percentage considered threatening the conservator must remove them.
See more ideas about metal salts ceramics ceramic sculpture.
If the ceramic is subjected to cycles of drying and wetting the salt compounds will crystallize and mobilize alternatively producing severe pressures on the ceramic body from within the pores ultimately.
I suppose it could almost be expected with backgrounds covering photography biology engineering chemistry music and graphics and a love of the outdoors that their work in ceramics would be organic technical.
In high humidity salts become soluble and in low humidity they crystallize.
The water dissolves the salt and draws it out of the ceramic.
This terra cotta clay vitrifies here at 1957f cone 03.
How bad can efflorescence of soluble salts of fired ceramic surfaces be.
This problem is common in many terra cotta materials but can also surface in others.
Soluble salt compounds may be introduced into the ceramic pores from ground water agricultural run off seawater or other sources.
Feb 16 2020 explore ceramic art community noticebo s board water soluble metal salt effects followed by 1601 people on pinterest.
Mark goudy and liza riddle are a couple from berkeley california who are blazing a new frontier in ceramic arts with their explorations into the applications of soluble metal salts.